The original zink plating experiment has evolved. To get the right chemicals (mainly the zink brightener) I surrended and bought them from Caswell.
I'm in the process of building the essential zinkplating rig at the moment. My intention was to start today but I did not have enough copper wires to complete it, maybe tomorrow.

This far I have made the rig for zinkplating the fork springs for the Fleetwood front fork (except the main zink anodes). In the picture below, at least the center anode...